Typical for MnZn and NiZn ferrites; Reproduced with permission from The Inductor Handbook
| Specific Heat |
0.25 cal/g/°C |
| Thermal Conductivity |
10 10−3 cal/sec/cm/°C |
Coefficient of Linear Expansion |
8 — 10 10−6/°C |
| Tensile Strength |
7 103 lbs/in2 |
| Compressive Strength |
60 103 lbs/in2 |
| Young Modulus |
18 103 lbs/in2 |
| Hardness (Knoop) |
650 |
| Specific Gravity |
≈4.7 g/cm3 |
|